水热腐蚀老化对热障涂层的摩擦磨损性能的影响 |
| 周文晖, 宋健, 陈泽浩, 杨兰兰, 王金龙, 陈明辉, 朱圣龙, 王福会 |
|
Effect of Low Temperature Degradation on Tribological Properties of YSZ Thermal Barrier Coatings |
| ZHOU Wenhui, SONG Jian, CHEN Zehao, YANG Lanlan, WANG Jinlong, CHEN Minghui, ZHU Shenglong, WANG Fuhui |
| 图8 H组试样反复相变示意图 |
| Fig.8 Schematic representations of phase transition of H group of samples (a) as-deposited coating; (b) water penetration in the ceramic top coating, the phase transformation of some YSZ grains from t-phase to m-phase happened, resulting in the volume expansion of the grains; (c) the m-phase transfomed to t-phase at high temperature and then the volume of the grains decreased. During this process, the accumulation of irreversible volume change induced the initiation of cracks |
|