温度对CO2饱和页岩气压裂液环境中N80和TP125V钢腐蚀行为影响研究 |
| 黄家和, 袁曦, 陈文, 闫文静, 金正宇, 柳海宪, 刘宏芳, 刘宏伟 |
|
Effect of Temperature on Corrosion Behavior of Pipeline Steels N80 and TP125V in Artificial CO2-saturated Fracturing Fluid of Shale Gas |
| HUANG Jiahe, YUAN Xi, CHEN Wen, YAN Wenjing, JIN Zhengyu, LIU Haixian, LIU Hongfang, LIU Hongwei |
| 图8 TP125V钢在不同温度下饱和CO2腐蚀测试介质中浸泡14 d后的极化曲线 |
| Fig.8 Polarization curves of TP125V steel after 14 d immersion in the CO2-saturated solution at different temperatures. |
|