温度对CO2饱和页岩气压裂液环境中N80和TP125V钢腐蚀行为影响研究 |
黄家和, 袁曦, 陈文, 闫文静, 金正宇, 柳海宪, 刘宏芳, 刘宏伟 |
Effect of Temperature on Corrosion Behavior of Pipeline Steels N80 and TP125V in Artificial CO2-saturated Fracturing Fluid of Shale Gas |
HUANG Jiahe, YUAN Xi, CHEN Wen, YAN Wenjing, JIN Zhengyu, LIU Haixian, LIU Hongfang, LIU Hongwei |
图4 在不同温度下饱和CO2腐蚀测试介质中浸泡14 d后N80钢和TP125V钢表面腐蚀产物XRD谱 |
Fig.4 XRD patterns of N80 steel (a) and TP125V steel (b) after 14 d immersion in the CO2-saturated solution at different temperatures |
![]() |