温度对CO2饱和页岩气压裂液环境中N80和TP125V钢腐蚀行为影响研究 |
黄家和, 袁曦, 陈文, 闫文静, 金正宇, 柳海宪, 刘宏芳, 刘宏伟 |
Effect of Temperature on Corrosion Behavior of Pipeline Steels N80 and TP125V in Artificial CO2-saturated Fracturing Fluid of Shale Gas |
HUANG Jiahe, YUAN Xi, CHEN Wen, YAN Wenjing, JIN Zhengyu, LIU Haixian, LIU Hongfang, LIU Hongwei |
图1 N80钢和TP125V钢在不同温度条件下饱和CO2腐蚀介质中浸泡14 d后由失重计算得到的腐蚀速率 |
Fig.1 Calculated corrosion rates of N80 steel (a) and TP125V steel (b) based on mass losses after immersion in the CO2-saturated solution for 14 d |
![]() |