干湿比对CrNiMoV钢在120 mmol/L NH4H2PO4溶液中电化学腐蚀行为的影响
王通, 孟惠民, 郭维华, 葛鹏飞, 巩秀芳, 倪荣, 龚显龙, 戴君, 隆彬, 李全德

Influence of Dry-wet Ratio on Electrochemical Corrosion Behavior of CrNiMoV Steel in 120 mmol/L NH4H2PO4 Solution
WANG Tong, MENG Huimin, GUO Weihua, GE Pengfei, GONG Xiufang, NI Rong, GONG Xianlong, DAI Jun, LONG Bin, LI Quande
表2 腐蚀产物膜中主要组成相的结合能
Table 2 Binding energies of the primary components in the corrosion product film
ElementPeakSpecies / binding energy
Fe2p3/2Fe3O4/709 eV; Fe2O3/711.5 eV; FeOOH/711.8 eV;Fe3(PO4)2/710.1 eV; FePO4/712.8 eV
Cr2p3/2CrO3/578.9 eV;Cr2O3/576 eV; Cr(OH)3/577.1 eV