垃圾焚烧电站水冷壁镍基合金涂层高温氯腐蚀性能研究 |
王永田, 赵祎璠, 魏啸天, 王嘉伟, 陈诚, 王宇, 张贝贝, 田欣利, 曲作鹏 |
High Temperature Chlorine Corrosion of Nickel Based Alloy Coating for Piping of Waste Incineration Power Plant |
WANG Yongtian, ZHAO Yifan, WEI Xiaotian, WANG Jiawei, CHEN Cheng, WANG Yu, ZHANG Beibei, TIAN Xinli, QU Zuopeng |
图4 试块经过600 ℃/400 h腐蚀后白色区域内的元素分布图 |
Fig.4 Corrosion image and element distribution after the test block was corroded at 600 ℃ for 400 h in white area |
![]() |