热处理工艺对超级13Cr不锈钢在饱和CO2油田地层水中腐蚀行为影响
潘鑫, 任泽, 连景宝, 何川, 郑平, 陈旭

Effect of Heat Treatment Process on Corrosion Behavior of Super 13Cr Stainless Steel in CO2-Saturated Oilfield Formation Aqueous Solution
PAN Xin, REN Ze, LIAN Jingbao, HE Chuan, ZHENG Ping, CHEN Xu
表3 不同条件热处理的超级13Cr不锈钢EIS拟合结果
Table 3 EIS fitting results of super 13Cr stainless steel of various heat treatment
Heat treatment conditionsRsΩ·cm-2RfΩ·cm-2CPEdlF·cm-2RctΩ·cm-2
quenching5.7329.409.74×10-66.38×104
550 ℃-tempering4.407.641.26×10-53.23×104
620 ℃-tempering4.7016.931.21×10-55.30×104
690 ℃-tempering4.523.221.79×10-52.69×104
Two-stage tempering5.3419.041.14×10-55.52×104