热处理工艺对超级13Cr不锈钢在饱和CO2油田地层水中腐蚀行为影响
潘鑫, 任泽, 连景宝, 何川, 郑平, 陈旭

Effect of Heat Treatment Process on Corrosion Behavior of Super 13Cr Stainless Steel in CO2-Saturated Oilfield Formation Aqueous Solution
PAN Xin, REN Ze, LIAN Jingbao, HE Chuan, ZHENG Ping, CHEN Xu
表1 超级13Cr不锈钢的热处理工艺
Table 1 Heat treatment processes of super 13Cr stainless steel
Sample numberHeat treatment condition
A1050 ℃×0.5 h oil cooling
B1050 ℃×0.5 h water cooling +550 ℃×6 h furnace cooled
C1050 ℃×0.5 h water cooling+620 ℃×6 h furnace cooled
D1050 ℃×0.5 h water cooling+690 ℃×6 h furnace cooled
E1050 ℃×0.5 h oil cooling+650 ℃×2 h furnace cooled+620 ℃×6 h furnace cooled