工业建筑屋面用铝锰合金的腐蚀行为
王嘉琪, 李莉, 刘婷婷

Corrosion Behavior of Al-Mn Alloys for Industrial Building Roof
WANG Jiaqi, LI Li, LIU Tingting
表4 不同状态Al-Mn-0.18RE合金在3.5%NaCl溶液中的极化曲线拟合结果
Table 4 Polarization curve fitting results of Al-Mn-0.18RE alloy with different states in 3.5%NaCl solution
State of sampleESCE / mVESCE / mV
Homogenization-694-634
Rolling-812-696
Cold rolling+325 ℃ annealing-801-694
Cold rolling+475 ℃ annealing-825-698