2.25Cr1Mo钢及其焊接接头在高温水蒸气中的应力腐蚀开裂敏感性研究 |
刘宇桐, 陈震宇, 朱忠亮, 冯瑞, 包汉生, 张乃强 |
SCC Susceptibility of 2.25Cr1Mo Steel and Its Weld Joints in High Temperature Steam |
LIU Yutong, CHEN Zhenyu, ZHU Zhongliang, FENG Rui, BAO Hansheng, ZHANG Naiqiang |
图3 水蒸气中的断口形貌SEM图 |
Fig.3 SEM images of the fracture surfaces of the test steel and its weld joints in steam environment: (a) test steel-2, (b) Z124-2, (c) Z125-2, (d) center and (e) edge regions for Z124-2 |
![]() |