高等级合金CO2环境下的腐蚀行为研究 |
| 梁志远, 徐一鸣, 王硕, 李玉峰, 赵钦新 |
|
Corrosion Behavior of Heat-resistant Alloys in High Temperature CO2 Environment |
| LIANG Zhiyuan, XU Yiming, WANG Shuo, LI Yufeng, ZHAO Qinxin |
| 图7 3种合金在不同温度下腐蚀100 h后的断面微观形貌 |
| Fig.7 Cross-sectional morphologies of Sanicro 25 steel (a), HR230 (b) and 740H (c) alloys after 100 h corrosion at 800 ℃ (a1-c1), 900 ℃ (a2-c2) and 1000 ℃ (a3-c3) |
|