高等级合金CO2环境下的腐蚀行为研究 |
梁志远, 徐一鸣, 王硕, 李玉峰, 赵钦新 |
Corrosion Behavior of Heat-resistant Alloys in High Temperature CO2 Environment |
LIANG Zhiyuan, XU Yiming, WANG Shuo, LI Yufeng, ZHAO Qinxin |
图6 3种材料在不同温度下腐蚀100 h后的表面微观形貌 |
Fig.6 Surface micromorphologies of Sanicro 25 steel (a), HR230 (b) and 740H (c) alloys after 800 ℃ (a1-c1), 900 ℃ (a2-c2) and 1000 ℃ (a3-c3) temperature corrosion at different temperatures for 100 h |
![]() |