高等级合金CO2环境下的腐蚀行为研究 |
梁志远, 徐一鸣, 王硕, 李玉峰, 赵钦新 |
Corrosion Behavior of Heat-resistant Alloys in High Temperature CO2 Environment |
LIANG Zhiyuan, XU Yiming, WANG Shuo, LI Yufeng, ZHAO Qinxin |
图5 3种材料在不同温度腐蚀100 h后的宏观表面形貌 |
Fig.5 Macro morphologies of 740H (a1-c1), HR230 (a2-c2) and Sanicro 25 (a3-c3) alloys after high temperature corrosion for 100 h at 800 ℃ (a), 900 ℃ (b) and 1000 ℃ (c) |
![]() |