高速列车铆接件中6A01铝合金腐蚀行为研究
陈志坚1, 周学杰1,2(), 陈昊1,3
Corrosion Behavior of Riveted Pair of 6A01 Al-alloy-/304 Stainless Steel-plate Used for High-speed Train
CHEN Zhijian1, ZHOU Xuejie1,2(), CHEN Hao1,3

图2. 不同盐雾时间后6组试样中6A01铝合金表面形貌

Fig.2. Surface morphologies of 6A01 Al-alloy after cyclic salt spray experiment for 10 d (a), 20 d (b), 30 d (c), 40 d (d), 50 d (e) and 60 d (f)