Cl-与HSO3-对建筑用439不锈钢腐蚀行为的影响
|
陈昊, 樊志彬, 陈志坚, 周学杰, 郑鹏华, 吴军
|
Effect of Cl- and HSO3- on Corrosion Behavior of 439 Stainless Steel Used in Construction
|
CHEN Hao, FAN Zhibin, CHEN Zhijian, ZHOU Xuejie, ZHENG Penghua, WU Jun
|
|
表2 循环极化曲线特征参数
|
Table 2 Characteristic parameters of cyclic polarization curves
|
|
Solution / mol·L-1 | Ecorr / V | Icorr / μA·cm-2 | Eb / V | Ep / V | Eb-Ep / V |
---|
0.62 NaCl | -0.071 | 0.119 | 0.320 | --- | --- | 0.05 NaHSO3 | -0.017 | 0.067 | 0.792 | 0.332 | 0.460 | 0.10 NaHSO3 | -0.073 | 0.101 | 0.779 | 0.321 | 0.459 | 0.50 NaHSO3 | -0.079 | 0.147 | 0.615 | 0.227 | 0.388 | (0.62+0.05) NaCl+NaHSO3 | -0.358 | 0.938 | -0.189 | -0.490 | --- | (0.62+0.10) NaCl+NaHSO3 | -0.282 | 0.613 | 0.258 | -0.491 | --- | (0.62+0.50) NaCl+NaHSO3 | -0.323 | 0.405 | 0.424 | -0.444 | --- |
|
|
|