湿气环境中抗硫钢的元素硫腐蚀特征及腐蚀机理
|
Characteristics and Mechanisms of Elemental Sulfur Induced Corrosion of Sulfur-resistant Steels in Wet Flow CO2 Environment
|
图8. 30%RH/60 ℃条件下覆盖物不含S时的P110SS钢表面去膜后形貌 |
Fig.8. SEM images of micro-morphologies of P110SS steel surface without elemental sulfur under 30%RH/60 ℃ |
![]() |