磷酸中核桃青皮复配缓蚀剂对冷轧钢的缓蚀协同效应
李向红1(), 徐昕1, 雷然1, 邓书端2
Synergistic Inhibition Effect of Walnut Green Husk Extract Complex Inhibitors on Steel in Phosphoric Acid
LI Xianghong1(), XU Xin1, LEI Ran1, DENG Shuduan2

图10. 冷轧钢浸泡前后的表面3D-AFM微观形貌

Fig.10. 3D-AFM surface micrographs of cold rolled steel before (a) and after immersion at 20 ℃ for 6 h in 2.0 mol/L H3PO4 solutions containing 0 mg/L inhibitor (b), 100 mg/L WGHE (c), 100 mg/L SLS (d) and 50 mg/L WGHE+50 mg/L SLS (e)