铝硅复合对Fe32Mn7Cr3Al2Si钢氧化改性层耐蚀性的影响 |
梁泰贺, 朱雪梅, 张振卫, 王新建, 张彦生 |
Corrosion Performance of Transition Layer at Interface of Oxide Scale/substrate Formed on Austenitic Steel Fe32Mn7Cr3Al2Si During High Temperature Oxidation |
LIANG Taihe, ZHU Xuemei, ZHANG Zhenwei, WANG Xinjian, ZHANG Yansheng |
图1 Fe32Mn7Cr3Al2Si钢固溶处理后微观组织EBSD像 |
Fig.1 EBSD image of Fe32Mn7Cr3Al2Si steel after solution treatment at 1273 K for 1 h |
![]() |