新型奥氏体不锈钢高温NaCl腐蚀行为研究 |
伊璞, 侯利锋, 杜华云, 刘笑达, 贾建文, 李阳, 张威, 徐芳泓, 卫英慧 |
NaCl Induced Corrosion of Three Austenitic Stainless Steels at High Temperature |
YI Pu, HOU Lifeng, DU Huayun, LIU Xiaoda, JIA Jianwen, LI Yang, ZHANG Wei, XU Fanghong, WEI Yinghui |
图4 3种不锈钢在不同温度下热腐蚀后的表面SEM图 |
Fig.4 SEM images of 254SMo (a~c), 904L (b~f) and 317L (g~i) stainless steels after hot corrosion at 750 ℃ (a, d, g), 850 ℃ (b, e, h) and 950 ℃ (c, f, i) for 60 h |
![]() |