新型奥氏体不锈钢高温NaCl腐蚀行为研究 |
伊璞, 侯利锋, 杜华云, 刘笑达, 贾建文, 李阳, 张威, 徐芳泓, 卫英慧 |
NaCl Induced Corrosion of Three Austenitic Stainless Steels at High Temperature |
YI Pu, HOU Lifeng, DU Huayun, LIU Xiaoda, JIA Jianwen, LI Yang, ZHANG Wei, XU Fanghong, WEI Yinghui |
图3 3种不锈钢在不同温度下腐蚀60 h前后的XRD图 |
Fig.3 XRD patterns of 254SMo (a), 904L (b) and 317L (c) stainless steels before and after hot corrosion for 60 h at different temperatures |
![]() |