新型奥氏体不锈钢高温NaCl腐蚀行为研究 |
| 伊璞, 侯利锋, 杜华云, 刘笑达, 贾建文, 李阳, 张威, 徐芳泓, 卫英慧 |
|
NaCl Induced Corrosion of Three Austenitic Stainless Steels at High Temperature |
| YI Pu, HOU Lifeng, DU Huayun, LIU Xiaoda, JIA Jianwen, LI Yang, ZHANG Wei, XU Fanghong, WEI Yinghui |
| 图1 3种不锈钢在不同温度下的腐蚀动力学曲线 |
| Fig.1 Mass losses of 254SMo, 904L and 317L stainless steels during hot corrosion at 750 ℃ (a), 850 ℃ (b) and 950 ℃ (c) |
|