超细层片结构Al-4%Cu合金的点蚀行为 |
辛叶春, 徐伟, 赵东杨, 张波 |
Pitting Corrosion Behavior of Ultra-fine Lamellated Al-4%Cu Alloy |
XIN Yechun, XU Wei, ZHAO Dongyang, ZHANG Bo |
图4 80 ℃时效过程显微硬度变化及不同时效时间后的组织 |
Fig.4 Variation of Vickers hardness of clod UFL Al-4%Cu at 80 ℃ with aging time (a), SEM-ECC images of UFL Al-4%Cu annealed for 0 h (b), 12 h (c) and 72 h (d) |
![]() |