铈离子修饰SiO2膜层在模拟深海条件下的腐蚀行为研究
窦建业, 屈少鹏, 轩星雨

Service Behavior of Cerium Ion Modified SiO2 Film Prepared by Different Methods in Artificial Deep Sea Environments
DOU Jianye, QU Shaopeng, XUAN Xingyu
表3 X80钢上溶胶-凝胶膜层和电沉积膜层在不同静水压3.5%NaCl溶液中的腐蚀电化学参数
Table 3 Electrochemical parameters of the sol-gel coating and electrodeposited coating on X80 steel in 3.5%NaCl solution under different hydrostatic pressures
SamplesEcorrVIcorrµA·cm-2βaV·dec-1βcV·dec-1
Sol-gel, 0.1 MPa-0.4341.580.09290.210
Sol-gel, 20 MPa-0.4346.570.08330.323
Electrodeposition, 0.1 MPa-0.5134.270.11090.158
Electrodeposition, 20 MPa-0.50417.480.06610.391