铜基超疏水表面的制备及其耐蚀性研究 |
| 尹续保, 李育桥, 高荣杰 |
|
Preparation of Superhydrophobic Surface on Copper Substrate and Its Corrosion Resistance |
| YIN Xubao, LI Yuqiao, GAO Rongjie |
| 图1 不同条件下处理后样品的表面形貌 |
| Fig.1 SEM surface images of Cu samples after chemical etching for 8 min (a), then oxidation at 160 ℃ for 6 h (b), finally 1-Dodecanethiol modification for 10 min (c), 15 min (d), 24 min (e) and 40 min (f) |
|