深海压力-流速耦合环境对环氧玻璃鳞片涂层失效行为的影响
高浩东, 崔宇, 刘莉, 孟凡帝, 刘叡, 郑宏鹏, 王福会

Influence of Simulated Deep Sea Pressured-flowing Seawater on Failure Behavior of Epoxy Glass Flake Coating
GAO Haodong, CUI Yu, LIU Li, MENG Fandi, LIU Rui, ZHENG Hongpeng, WANG Fuhui
图17 4种环境下浸泡120 h以后涂层拉伸断口微观形貌
Fig.17 SEM images of the coating tensile fracture after immersing for 120 h under different environment: (a) 0.1 MPa-0 m/s, (b) 10 MPa-0 m/s, (c) 0.1 MPa-4 m/s, (d) 10 MPa-4 m/s