深海压力-流速耦合环境对环氧玻璃鳞片涂层失效行为的影响
高浩东, 崔宇, 刘莉, 孟凡帝, 刘叡, 郑宏鹏, 王福会

Influence of Simulated Deep Sea Pressured-flowing Seawater on Failure Behavior of Epoxy Glass Flake Coating
GAO Haodong, CUI Yu, LIU Li, MENG Fandi, LIU Rui, ZHENG Hongpeng, WANG Fuhui
图14 10 MPa-4 m/s环境下浸泡120 h后涂层表面的EDS分析
Fig.14 Coating surface image (a) and EDS maps (b, c) after 120 h immersion in 10 MPa-4 m/s environment