深海压力-流速耦合环境对环氧玻璃鳞片涂层失效行为的影响 |
高浩东, 崔宇, 刘莉, 孟凡帝, 刘叡, 郑宏鹏, 王福会 |
Influence of Simulated Deep Sea Pressured-flowing Seawater on Failure Behavior of Epoxy Glass Flake Coating |
GAO Haodong, CUI Yu, LIU Li, MENG Fandi, LIU Rui, ZHENG Hongpeng, WANG Fuhui |
图13 4种环境中浸泡120 h以后涂层表面的SEM像 |
Fig.13 SEM images of the coating surface after immersing for 120 h under different environment: (a) 0.1 MPa-0 m/s, (b) 10 MPa-0 m/s, (c) 0.1 MPa-4 m/s, (d) 10 MPa-4 m/s |
![]() |