深海压力-流速耦合环境对环氧玻璃鳞片涂层失效行为的影响 |
高浩东, 崔宇, 刘莉, 孟凡帝, 刘叡, 郑宏鹏, 王福会 |
Influence of Simulated Deep Sea Pressured-flowing Seawater on Failure Behavior of Epoxy Glass Flake Coating |
GAO Haodong, CUI Yu, LIU Li, MENG Fandi, LIU Rui, ZHENG Hongpeng, WANG Fuhui |
图11 干态及4种环境下浸泡120 h后样品的宏观形貌 |
Fig.11 Macro morphologies of the coating after immersion for 120 h in dry (a), 0.1 MPa-0 m/s (b), 10 MPa-0 m/s (c), 0.1 MPa-4 m/s (d) and 10 MPa-4 m/s (e) |
![]() |