5083铝合金与30CrMnSiA钢在不同Cl-浓度中电偶腐蚀行为的研究 |
||||||||||||||||||||
刘泉兵, 刘宗德, 郭胜洋, 肖毅 | ||||||||||||||||||||
Galvanic Corrosion Behavior of 5083 Al-alloy and 30CrMnSiA Steel in NaCl solutions |
||||||||||||||||||||
LIU Quanbing, LIU Zongde, GUO Shengyang, XIAO Yi | ||||||||||||||||||||
表2 在不同Cl-浓度溶液中浸泡15 d后的电偶对中铝合金腐蚀区域的EDS分析结果 |
||||||||||||||||||||
Table 2 EDS analysis results of the corrosion products formed on 5083Al-alloy in the couple after 15 d immersion in the NaCl solutions with different concentrations (mass fraction / %) |
||||||||||||||||||||
|
||||||||||||||||||||