Q235钢在氧化性含Cl气氛中的高温腐蚀行为
陈土春1, 向军淮1(), 江龙发2, 熊剑3, 白凌云1, 徐勋虎1, 徐鑫成1
High-temperature Corrosion Behavior of Q235 Steel in Oxidizing Atmosphere Containing Chlorine
CHEN Tuchun1, XIANG Junhuai1(), JIANG Longfa2, XIONG Jian3, BAI Lingyun1, XU Xunhu1, XU Xincheng1

图3. Q235钢在500和600 ℃腐蚀64 h后的XRD谱

Fig.3. XRD patterns of Q235 steel after corrosion at 500 and 600 ℃ for 64 h