T/S-52K直缝钢在不同Cl-浓度下的腐蚀行为
|
Corrosion Behavior of T/S-52K Straight Seam Pipeline Steel in Solutions of Different NaCl Concentration
|
图5. T/S-52K直缝钢试样在80 ℃下不同浓度的NaCl溶液中浸泡72 h后的电化学阻抗图谱及其等效电路 |
Fig.5. EIS (a~c) and corresponding equivalent circuit diagrams (d~f) of T/ S-52K pipeline steel after immersion for 72 h in 8 g/L (a, d), 20 g/L (b, e) and 35 g/L (c, f) NaCl solutions |
![]() |