表1 气井全生命周期环境的腐蚀介质特征
|
Table 1 Characteristics of gas well full-life-cycle environment
|
|
Full-life-cycle environment | Composition / mg·L-1 | pH | Temperature / ℃ | Time |
---|
Live acid (LA) | 10%HCl+1.5%HF+3%HAc+5%TG201 corrosion inhibitor | 10%~20% acid solution | 120 | 4 h | Spent acid (SA) | K+ / 1597.32, Ca2+ / 11693.00, Mg2+ / 3145.63, Cl- / 62738.01, Fe2+/52.40 | 2.6 | 180 | 5 d | Condensate water (CW) | K+ / 7380, Ca2+ / 4.745, Mg2+ / 2.463, Na+ / 1050,HCO3- / 4310, Cl- / 2990, SO42- / 862 | 7.79 | 180 | 10 d | Formation water (FW) | K+ / 6620, Ca2+ / 8310, Mg2+ / 561, Na+ / 76500, HCO3- / 189, Cl- / 128000, SO42- / 430 | 6.98 | 180 | 15, 30, 60 and 90 d |
|
|
|