湖南地区大气腐蚀严酷性的环境因素与大气腐蚀监测仪评定
王军1, 陈军君1, 谢亿1, 徐松1, 刘兰兰2, 吴堂清3(), 尹付成3
Evaluation of Environmental Factors Related with Atmosphere Corrosivity in Hunan Provice by Atmospheric Corrosion Monitoring Technique
WANG Jun1, CHEN Junjun1, XIE Yi1, XU Song1, LIU Lanlan2, WU Tangqing3(), YIN Fucheng3

图4. 2、3、10、14号试验点中Q235平板钢,Q345平板钢和Q235角钢年腐蚀深度随时间的演化

Fig.4. Variations of the corrosion depth of Q235 flat steel (a), Q345 flat steel (b) and Q235 angle steel (c) in 2#, 3#, 10# and 14# stations with exposure time