湖南地区大气腐蚀严酷性的环境因素与大气腐蚀监测仪评定
王军1, 陈军君1, 谢亿1, 徐松1, 刘兰兰2, 吴堂清3(), 尹付成3
Evaluation of Environmental Factors Related with Atmosphere Corrosivity in Hunan Provice by Atmospheric Corrosion Monitoring Technique
WANG Jun1, CHEN Junjun1, XIE Yi1, XU Song1, LIU Lanlan2, WU Tangqing3(), YIN Fucheng3

图1. Q235平板钢、Q345平板钢和Q235角钢在14个站点的年腐蚀深度

Fig.1. Annual corrosion depths of Q235 flat steel, Q345 flat steel and Q235 angle steel in 14 stations after 1 a exposure