O3/SO2复合大气环境中Q235B钢的腐蚀演化特性
|
Corrosion Evolution Characteristics of Q235B Steel in O3/SO2 Composite Atmosphere
|
图3. Q235B钢在模拟大气中经过30 CCT后腐蚀产物的XRD谱 |
Fig.3. XRD patterns of the powdered rust Q235B steel after 30 CCT in the simulated atmospheres: (a) 1# sample, (b) 2# sample, (c) 3# sample |
![]() |