低合金耐热钢T23在高温超临界CO2环境中的腐蚀特性研究
李瑞涛, 肖博, 刘晓, 朱忠亮, 程义, 李俊菀, 曹杰玉, 丁海民, 张乃强

Corrosion Behavior of Low Alloy Heat-resistant Steel T23 in High-temperature Supercritical Carbon Dioxide
LI Ruitao, XIAO Bo, LIU Xiao, ZHU Zhongliang, CHENG Yi, LI Junwan, CAO Jieyu, DING Haimin, ZHANG Naiqiang
图5 氧化时长1000 h试样 (2#试样) 表面氧化皮剥落位置区域1的氧化物形貌
Fig.5 Surface morphology of location 1 formed on T23 sample (2#) after exposing to high-temperature s-CO2 at 650 ℃ under 25 MPa for 1000 h (a) and higher magnification view for a small part (black box) of this area (b)