铝镁双金属反向等温包覆挤压棒材耐腐蚀性能
乔及森, 夏宗辉, 刘立博, 许佳敏, 刘旭东

Corrosion Resistance of Aluminum-magnesium Bimetal Composite Material Prepared by Isothermal Indirect Extrusion
QIAO Jisen, XIA Zonghui, LIU Libo, XU Jiamin, LIU Xudong
表3 材料在3.5%NaCl溶液中腐蚀前后的开路电位 (V)
Table 3 Open circuit potential of materials before and after corrosion in 3.5%NaCl solution
MaterialBefore corrosionAfter corrosion
2A12-0.9731-0.1742
2A12/AZ31-1.039-0.2789
Intreface layer-1.570-0.5639
AZ31(ES)-1.591-0.7169
AZ31(BS)-1.600-1.498