交变应力频率对E690钢在3.5%NaCl溶液中腐蚀电化学行为的影响
张腾, 刘静(), 黄峰, 胡骞, 戈方宇
Effect of Alternating Stress Frequency on Corrosion Electrochemical Behavior of E690 Steel in 3.5%NaCl Solution
ZHANG Teng, LIU Jing(), HUANG Feng, HU Qian, GE Fangyu

图7. E690钢在3.5%NaCl溶液中不同加载频率下腐蚀24 h后的表面形貌