电化学充氢对Cr15铁素体不锈钢和304奥氏体不锈钢氢脆敏感性的影响
张慧云1,2, 郑留伟1,3, 孟宪明2, 梁伟1,3()
Effect of Electrochemical Hydrogen Charging on Hydrogen Embrittlement Sensitivity of Cr15 Ferritic and 304 Austenitic Stainless Steels
ZHANG Huiyun1,2, ZHENG Liuwei1,3, MENG Xianming2, LIANG Wei1,3()

图9. 充氢后304奥氏体不锈钢断口形貌

Fig.9. Fracture morphologies of 304 stainless steel after hydrogen charging: general view (a) and enlarged views in the corner (I) (b), transition zone (II) (c) and center (III) (d)