pH对14Cr12Ni3WMoV不锈钢在含氯溶液中腐蚀行为的影响
冉斗, 孟惠民, 刘星, 李全德, 巩秀芳, 倪荣, 姜英, 龚显龙, 戴君, 隆彬

Effect of pH on Corrosion Behavior of 14Cr12Ni3WMoV Stainless Steel in Chlorine-containing Solutions
RAN Dou, MENG Huimin, LIU Xing, LI Quande, GONG Xiufang, NI Rong, JIANG Ying, GONG Xianlong, DAI Jun, LONG Bin
表3 钝化膜中主要组成物质的结合能
Table 3 Binding energies of the primary compounds of passive film
ElementPeakSpecies/binding energy
Fe2p3/2Fe/706.5 eV; FeO/709.9 eV; Fe3O4/708.2 eV; Fe2O3/711.5 eV; FeOOH/712 eV
Cr2p3/2Cr/573.8 eV; Cr2O3/576.0 eV; Cr(OH)3/577.0 eV; CrO3/578.3 eV
Mo3d5/2Mo/227.4 eV; Mo4+/228.8 eV; Mo6+/232.3 eV
3d3/2Mo/231.1 eV; Mo4+/234.2 eV;Mo6+/235.6 eV
W4f7/2W/31.0 eV; W6+/35.2 eV
4f5/2W/33.6 eV; W6+/37.4 eV