pH对14Cr12Ni3WMoV不锈钢在含氯溶液中腐蚀行为的影响
冉斗1,2, 孟惠民1, 刘星1,2, 李全德1,2,3(), 巩秀芳2,3, 倪荣2,3, 姜英2,3, 龚显龙2,3, 戴君2,3, 隆彬2,3()
Effect of pH on Corrosion Behavior of 14Cr12Ni3WMoV Stainless Steel in Chlorine-containing Solutions
RAN Dou1,2, MENG Huimin1, LIU Xing1,2, LI Quande1,2,3(), GONG Xiufang2,3, NI Rong2,3, JIANG Ying2,3, GONG Xianlong2,3, DAI Jun2,3, LONG Bin2,3()

图6. 14Cr12Ni3WMoV不锈钢在不同pH下0.1 mol/L NaCl溶液中点蚀坑的深度和孔径

Fig.6. Depth and aperture of the pitting of 14Cr12Ni3-WMoV stainless steel in 0.1 mol/L NaCl solution at different pH