硫酸盐还原菌作用下2205双相不锈钢在3.5%NaCl溶液中应力腐蚀开裂行为研究
|
Stress Corrosion Cracking Behavior of 2205 Duplex Stainless Steel in 3.5%NaCl Solution with Sulfate Reducing Bacteria
|
图7. 2205DSS在不同条件下主断口和侧断口形貌 |
Fig.7. Main fracture (a1~e1) and side fracture (a2~e2) morphologies of 2205DSS immersed in sterile solution (a1, a2) and bacteria containing solution for 3 d (b1, b2), 8 d (c1, c2), 10 d (d1, d2) and 14 d (e1, e2) |
![]() |