硫酸盐还原菌作用下2205双相不锈钢在3.5%NaCl溶液中应力腐蚀开裂行为研究
王欣彤, 陈旭(), 韩镇泽, 李承媛, 王岐山
Stress Corrosion Cracking Behavior of 2205 Duplex Stainless Steel in 3.5%NaCl Solution with Sulfate Reducing Bacteria
WANG Xintong, CHEN Xu(), HAN Zhenze, LI Chengyuan, WANG Qishan

图6. SSRT后2205DSS伸长率和断面收缩率的变化曲线

Fig.6. Elongation (a) and reduction of area (b) curves of 2205DSS after SSRT