Q235钢/导电混凝土在3种典型土壤环境中腐蚀的灰色关联度分析
唐荣茂, 朱亦晨, 刘光明, 刘永强, 刘欣, 裴锋

Gray Correlative Degree Analysis of Q235 Steel/conductive Concrete Corrosion in Three Typical Soil Environments
TANG Rongmao, ZHU Yichen, LIU Guangming, LIU Yongqiang, LIU Xin, PEI Feng
表5 Q235钢腐蚀电流密度和土壤环境因素相关序列
Table 5 Correlated sequence of Q235 steel corrosion current density and soil environmental factors
SequenceX0X1X2X3X4X5X6X7
symbolIcorr / A·cm-2Ca2+ / mmol·L-1Mg2+ / mmol·L-1Fe3+ / mmol·L-1Cl- / mmol·L-1SO42- / mmol·L-1HCO3- / mmol·L-1pH
Saline-alkali soil3.770×10-70.25001.43501.31250.71000.31007.69008.02
Yellow brown soil3.819×10-70.12160.13170.12120.17600.41001.26007.84
Red soil2.752×10-60.06150.06460.00860.10000.33800.42004.97