热带海洋大气环境中EH36船板钢早期腐蚀行为研究
李子运1, 王贵1, 罗思维1, 邓培昌2, 胡杰珍1(), 邓俊豪1, 徐敬明1
Early Corrosion Behavior of EH36 Ship Plate Steel in Tropical Marine Atmosphere
LI Ziyun1, WANG Gui1, LUO Siwei1, DENG Peichang2, HU Jiezhen1(), DENG Junhao1, XU Jingming1

图4. EH36船板钢暴露180 d后锈层截面腐蚀形貌和元素分布

Fig.4. Corrosion morphologies (a) and element distribution (b~f) of the cross section of EH36 ship steel after exposed for 180 d