热带海洋大气环境中EH36船板钢早期腐蚀行为研究
李子运1, 王贵1, 罗思维1, 邓培昌2, 胡杰珍1(), 邓俊豪1, 徐敬明1
Early Corrosion Behavior of EH36 Ship Plate Steel in Tropical Marine Atmosphere
LI Ziyun1, WANG Gui1, LUO Siwei1, DENG Peichang2, HU Jiezhen1(), DENG Junhao1, XU Jingming1

图2. EH36船板钢暴露不同时间后表面宏观形貌

Fig.2. Macroscopic surface morphologies of EH36 ship plate steel after exposed for 15 d (a), 30 d (b), 90 d (c), 180 d (d) and 360 d (e)