冷拉拔变形过程中含稀土铝镁合金腐蚀行为研究
张欣1,2(), 杨光恒1, 王泽华1, 曹静1, 邵佳1, 周泽华1
Corrosion Behavior of Al-Mg-RE Alloy Wires Subjected to Different Cold Drawing Deformation
ZHANG Xin1,2(), YANG Guangheng1, WANG Zehua1, CAO Jing1, SHAO Jia1, ZHOU Zehua1

图7. 铸态Al-3.0%Mg-0.12%RE合金在3.5%NaCl溶液中浸泡21 d后合金表面形貌和EDS分析

Fig.7. Surface morphologies (a, b) and EDS analysis (c, d) of as-cast Al-3.0%Mg-0.12%RE alloys after the 21 d immersion test in 3.5%NaCl solution