冷拉拔变形过程中含稀土铝镁合金腐蚀行为研究
张欣1,2(), 杨光恒1, 王泽华1, 曹静1, 邵佳1, 周泽华1
Corrosion Behavior of Al-Mg-RE Alloy Wires Subjected to Different Cold Drawing Deformation
ZHANG Xin1,2(), YANG Guangheng1, WANG Zehua1, CAO Jing1, SHAO Jia1, ZHOU Zehua1

图4. 铸态Al-3.0%Mg-0.12%RE合金微观组织形貌与EDS元素分析

Fig.4. Optical image (a), SEM image (b) and EDS analysis of Fe (c), Al (d), Mg (e), Ce (f) and La (g) of Al-3.0%Mg-0.12%RE alloy