X65管线钢在油水两相界面处的CO2腐蚀行为研究
贾巧燕1, 王贝1, 王赟1, 张雷1(), 王清2, 姚海元2, 李清平2, 路民旭1
Corrosion Behavior of X65 Pipeline Steel at Oil-Water Interface Region in Hyperbaric CO2 Environment
JIA Qiaoyan1, WANG Bei1, WANG Yun1, ZHANG Lei1(), WANG Qing2, YAO Haiyuan2, LI Qingping2, LU Minxu1

图4. X65钢在加入100 mg/L癸硫醇的油水两相界面区域腐蚀沟槽形貌

Fig.4. Enlarged morphologies of corrosion groove of X65 steel in oil-water interface region with 100 mg/L decyl mercaptan: (a) macro corrosion morphology, (b) micro corrosion morphologies 3D profile, (c) depth curve of guttering corrosion