垃圾焚烧锅炉关键受热面腐蚀研究进展及方向思考
|
Research Progress and Direction Thinking on Corrosion of Key Heat Transfer Components in Waste Incineration Boilers
|
图2. 在He±5%O2±815 mg/m3 HCl中400~700 ℃下Fe的腐蚀的热重分析结果[ |
Fig.2. Thermogravimetric results for the corrosion of iron at 400~700 ℃ in He±5% O2±815 mg/m3 HCl[ |
![]() |